Lubrizol Advanced Materials PEARLBOND® DIPP-539 Linear Thermoplastic Polyurethane  (discontinued **)

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLBOND® DIPP-539 Linear Thermoplastic Polyurethane  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PEARLBOND® DIPP-539 is a linear, polycaprolactone-copolester polyurethane with a very high crystallization rate and a very high thermoplasticity level.Applications: PEARLBOND® DIPP-539 can be added to formulations of REACTIVE POLYURETHANE HOT-MELTS, in order to improve the crystallisation speed.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
DIN 53.479
Viscosity 170000 cP

@Temperature 130 °C
170000 cP

@Temperature 266 °F
Melt; DIN 53.735
Melt Flow 150 - 200 g/10 min

@Load 2.16 kg,
Temperature 170 °C
150 - 200 g/10 min

@Load 4.76 lb,
Temperature 338 °F
DIN 53.735
Thermal Properties Metric English Comments
Melting Point 58.0 - 60.0 °C
136 - 140 °F
MQSA 70 A
Chemical Properties Metric English Comments
Total Base Number <= 5.0
<= 5.0
mg KOH/g; MQSA 47
Processing Properties Metric English Comments
Moisture Content <= 0.15 %
<= 0.15 %
MQSA 44
Descriptive Properties Value Comments
Crystallization rate (minutes) 8 - 10
MQSA 12 B
Supply Form Small white pellets
Thermoplasticity Very high
MQSA 68 A