Lubrizol Advanced Materials Pearlstick® 45-40/03 Polycaprolactone based TPU  (discontinued **)

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials Pearlstick® 45-40/03 Polycaprolactone based TPU  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TPUs for Solvent-based adhesivesApplications: Automotive, OthersInformation provided by Merquinsa
Physical Properties Metric English Comments
Viscosity 200 - 400 cP
200 - 400 cP
15% solution in MEK
Processing Properties Metric English Comments
Processing Temperature 45.0 °C
113 °F
Min. Activation Temp; EN 12961
Descriptive Properties Value Comments
Crystallization Rate (MQSA n° 12 A) VERY HIGH
Solubility - Acetone / Ethyl Acetate 30:70
Solubility - Acetone / Toluene 35:65
Solubility - MEK / Toluene 60:40
Solubility - MEK/ Ethyl Acetate 40:60
Thermoplasticity Range (MQSA n° 58) MEDIUM