Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Processing Temperature = 113 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 45.0 - 249 °C
113 - 480 °F
Average value: 171 °C Grade Count:5
Overview of materials for PETG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
Processing Temperature 45.0 °C
113 °F
Min. Activation Temp; EN 12961
Lubrizol Advanced Materials Pearlstick® 45-40/05 Polycaprolactone based TPU  (discontinued **)
TPUs for Solvent-based adhesivesApplications: DIY, AutomotiveInformation provided by Merquinsa
Processing Temperature 45.0 °C
113 °F
Min. Activation Temp; EN 12961
Lubrizol Advanced Materials Pearlstick® 45-40/11S Polycaprolactone based TPU  (discontinued **)
TPUs for Solvent-based adhesivesApplications: ShoeInformation provided by Merquinsa
Processing Temperature 45.0 °C
113 °F
Min. Activation Temp; EN 12961
Lubrizol Advanced Materials Pearlstick® 45-40/08 Polycaprolactone based TPU
Pearlstick 45-40/08 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a medium thermoplasticity level. Solubility..
Processing Temperature 45.0 °C
113 °F
Min. Activation Temp; EN 12961
Lubrizol Advanced Materials Pearlstick® 45-40/27 Polycaprolactone based TPU
Pearlstick 45-40/27 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a medium thermoplasticity level.Solubility:..
Processing Temperature 45.0 °C
113 °F
Roll 1 Temperature
SK Chemicals SKYGREEN® PETG 2008 Specially Formulated PET Copolymer Resin
SKYGREEN PETG is an amorphous copolyester in which a certain amount of ethylene glycol is replaced with 1,4-cyclohexane dimethanol (CHDM), which prevent crystallization, leading to improved processa..
Processing Temperature 45.0 °C
113 °F
Min. Activation Temp; EN 12961
Lubrizol Advanced Materials Pearlstick® 45-40/03 Polycaprolactone based TPU  (discontinued **)
TPUs for Solvent-based adhesivesApplications: Automotive, OthersInformation provided by Merquinsa
Processing Temperature 45.0 °C
113 °F
Min. Activation Temp; EN 12961
Lubrizol Advanced Materials Pearlstick® 45-40/15 Polycaprolactone based TPU
Pearlstick 45-40/15 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a medium thermoplasticity level. Solubility: ..
Processing Temperature 45.0 °C
113 °F
Min. Activation Temp; EN 12961
Lubrizol Advanced Materials Pearlstick® 45-40/19 Polycaprolactone based TPU
Pearlstick 45-40/19 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a medium thermoplasticity level.Solubility: P..
Copyright © lookpolymers.com All Rights Reserved