Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Advanced Materials Pearlstick® 45-80/16 Polycaprolactone based TPU

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlstick®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials Pearlstick® 45-80/16 Polycaprolactone based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pearlstick 45-80/16 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a small amount of anti-adherent in the formulation. It has a very low crystallization rate and very low thermoplasticity level. Pearlstick 45-80/16 is adequate for bonding processes that do not require heat activation (cold bonding).Solubility: Pearlstick 45-80/16 is soluble in Acetone, Methyl Ethyl Ketone (MEK), Cyclohexanone, Dimethyl Formamide, and Tetrahydrofurane (THF). The solvents and diluents should be water-free (max. 0.1 %), so as to avoid subsequent side reactions during crosslinking with isocyanate. It should be dissolved in closed tanks, and the use of a variable speed agitator is advisable. The final viscosity fies can vary, depending on the stirring process and on the solvent/diluents ratios Applications: Pearlstick 45-80/16 is used for the production of adhesives for different kinds of materials such as leather, textiles, rubber and a variety of plastics (plasticized PVC, PU elastomers, etc.). Pearlstick 45-80/16 allows the production of adhesives with a very long open-time, which can be used without requiring heat activation. The addition of Pearlstick 45-80/16 to other different types of Pearlstick increases their open-times. The addition of a polyfunctional isocyanate to improves the heat-resistance and the strength of the joints.Information provided by Merquinsa
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 2781
Brookfield Viscosity 1400 - 1800 cP
1400 - 1800 cP
Brookfield RVF sp 4, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A
Descriptive Properties Value Comments
Crystallization Rate (MQSA n° 12 A) LOW
Hydrolysis Resistance Good
MQSA 34B
Hydroxyl Number 0.1%
MQSA 47A
Solubility - Acetone / Ethyl Acetate 85:15
Solubility - Acetone / Toluene 70:30
Solubility - MEK / Toluene 90:10
Solubility - MEK/ Ethyl Acetate 90:10
Thermoplasticity Range (MQSA n° 58) LOW