Lubrizol Advanced Materials Pearlstick® 45-90/16 Polycaprolactone based TPU  (discontinued **)

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials Pearlstick® 45-90/16 Polycaprolactone based TPU  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TPUs for Solvent-based adhesivesApplications: Automotive, Others, ShoeInformation provided by Merquinsa
Physical Properties Metric English Comments
Viscosity 1400 - 1800 cP
1400 - 1800 cP
15% solution in MEK
Processing Properties Metric English Comments
Processing Temperature 40.0 °C
104 °F
Min. Activation Temp; EN 12961
Descriptive Properties Value Comments
Crystallization Rate (MQSA n° 12 A) LOW
Solubility - Acetone / Ethyl Acetate 85:15
Solubility - Acetone / Toluene 70:30
Solubility - MEK / Toluene 90:10
Solubility - MEK/ Ethyl Acetate 90:10
Thermoplasticity Range (MQSA n° 58) LOW