Lubrizol Advanced Materials Pearlstick® 49-46/23 Linear Thermoplastic Polyurethane Elastomer  (discontinued **

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials Pearlstick® 49-46/23 Linear Thermoplastic Polyurethane Elastomer  (discontinued **.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pearlstick 49-46/23 is an elastic, linear, aromatic polyurethane with a very high crystallization rate and a low thermoplasticity level, available as pellets.Solubility: Pearlstick 49-46/23 is soluble in acetone, methyl ethyl ketone (MEK), cyclohexanone, dimethyl formamide and tetrahydrofuran (THF). Diluting solvents such as toluene and ethyl acetate can be added.The solvents and diluents should be water-free (max 0.1%), so as to avoid subsequent side reactions during crosslinking with isocyanates.Solutions: Pearlstick 49-46/23 gives transparent solutions. It should be dissolved in closed tanks, and the use of high shear equipment is advised. The final viscosity fies can vary, depending on the stirring process and on the solvent/diluents ratios.Applications: Pearlstick 49-46/23 is used for the production of adhesives for bonding plasticized PVC to plasticized PVC or other materials such as leather, textiles, rubber, in the shoe industry. The addition of a poly-functional isocyanate improves the performance of the adhesive.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
Brookfield Viscosity 2100 - 2500 cP

@Temperature 20.0 °C
2100 - 2500 cP

@Temperature 68.0 °F
Brookfield RVF sp. 4, 20 rpm solution at 15% in MEK; MQSA N° 40A
Processing Properties Metric English Comments
Processing Temperature >= 65.0 °C
>= 149 °F
Activation Temperature
Descriptive Properties Value Comments
Color white or slightly yellowish
Crystallization Rate Very High
Freezing Resistance Very good
MQSA N° 90
Heat Resistance Excellent
Hydroxyl Content Approx. 0.1%
Thermoplasticity Range Low