Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Advanced Materials Pearlthane® ECO 12T95 Thermoplastic Polyurethane

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials Pearlthane® ECO 12T95 Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type : Pearlthane® ECO 12T95 is a high performance bio-based thermoplastic polyurethane. With ca. 32% bio-based content.Main Application : Injection MouldingSpecial Features : Excellent mechanical properties and abrasion resistance.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ISO 2781
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ISO 868
Tensile Strength 35.99 MPa
5220 psi
ISO 527-2/5A/500
Elongation at Break 415 %
415 %
ISO 527-2/5A/500
50% Modulus 0.0100 GPa
1.45 ksi
ISO 527-2/5A/500
100% Modulus 0.0120 GPa
1.74 ksi
ISO 527-2/5A/500
300% Modulus 0.0280 GPa
4.06 ksi
ISO 527-2/5A/500
Tear Strength 142 kN/m
811 pli
ISO 34-1B
Abrasion 28
28
mm<sup>3</sup> Loss; ISO 4649-A
Thermal Properties Metric English Comments
Vicat Softening Point 107 °C
225 °F
ISO 306
Processing Properties Metric English Comments
Feed Temperature 40.0 °C
104 °F
Nozzle Temperature 215 - 225 °C
419 - 437 °F
Zone 1 200 - 210 °C
392 - 410 °F
Zone 2 205 - 215 °C
401 - 419 °F
Zone 3 210 - 220 °C
410 - 428 °F
Zone 4 210 - 220 °C
410 - 428 °F
Dry Time 3.00 hour

@Temperature 100 °C
3.00 hour

@Temperature 212 °F
Descriptive Properties Value Comments
Biobased Content (%) 32
Compression Zone Temperature 401°F
Metering Zone Temperature 410°F