Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 107 °C @Load 1.00 kg |
225 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Clearflex® FG 308 Octene Copolymer Linear Low Density Polyethylene Clearflex FG 308 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 308 ar.. |
|||
Vicat Softening Point | 107 °C | 225 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® C6600 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Vicat Softening Point | 107 °C | 225 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics GELOY XP4025 ASA (Europe-Africa-Middle East) GELOY XP4025 is a high heat modified ASA/PC blend, for automotive exterior applications. It shows very good properties, gloss and colour retention, as well as faster cycle time over competitive mate.. |
|||
Vicat Softening Point | 107 °C | 225 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® DMX9254 PC Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Vicat Softening Point | 107 °C | 225 °F | ASTM D1525 |
Plaskolite West Optix® CA-71 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. High heat resistance, medium flow. |
|||
Vicat Softening Point | 107 °C | 225 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics GELOY XP7560 ASA (Europe-Africa-Middle East) GELOY XP7560 is a general purpose ASA/PC injection moulding grade, available in various colours. |
|||
Vicat Softening Point | 107 °C | 225 °F | 50°C/hr; 50N |
Polimeri Europa KOBLEND PCA PD 55 PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABS Halogen free injection moulding grade with flame retardant properties ( UL 94 V-0 at 1.6mm thickness ). Main application fields: business machines, electroni.. |
|||
Vicat Softening Point | 107 °C | 225 °F | 50°C/hr; 50N |
Polimeri Europa SINKRAL C350 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-08-16-25 Heat resistant injection moulding grade. Combines good flow with toughness and high thermal charac.. |
|||
Vicat Softening Point | 107 °C | 225 °F | ASTM D1525 |
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 8% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Vicat Softening Point | 107 °C | 225 °F | ASTM D1525 |
Huntsman IROGRAN® PS 443-201 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
Vicat Softening Point | 107 °C | 225 °F | ISO 306A |
Lucite International Diakon® ST50G8 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Vicat Softening Point | 107 °C | 225 °F | VST B50; ISO 306 |
Styrolution Luran® 378 P Crystal Clear Transparent SAN Description: Easy-flow grade with enhanced resistance to chemicals.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Vicat Softening Point | 107 °C | 225 °F | B/120; ISO R306 |
Samsung Cheil Industries Starex® GR-5020T SAN, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 107 °C | 225 °F | ISO 306/B50 |
Styron MAGNUMâ„¢ 3416 SLG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines excellent processability with a stable light base color providing an ideal resin for self coloring.. |
|||
Vicat Softening Point | 107 °C | 225 °F | |
Styron Magnum™ 9030 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Vicat Softening Point | 107 °C | 225 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Europe-Africa-Middle East) PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed. |
|||
Vicat Softening Point | 107 °C | 225 °F | |
Styron Magnum™ 1040 ABS, Very High impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Vicat Softening Point | 107 °C | 224 °F | ASTM D1525 |
Total PSC 585 Polystyrene Polystyrene 585 is a high molecular weight, low melt flow, crystal polystyrene. This polymer is tailored for extruded foam applications such as egg cartons, meat trays and food service. 585 also mak.. |
|||
Vicat Softening Point | 107 °C | 225 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D1525 |
Eastman Tenite Propionate 383A2R30007 Natural, Trsp Cellulose Acetate Propionate Plasticizer 7%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Vicat Softening Point | 107 °C | 224 °F | 0.125 inch, 1 Kg; ASTM D1525 |
Diamond Polymers ABS 3501 Natural 1000 P Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Vicat Softening Point | 107 °C | 224 °F | 0.125 inch, 1 Kg; ASTM D1525 |
Diamond Polymers ABS 3501E Natural 1000 S Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Vicat Softening Point | 107 °C | 224 °F | Rate A (50°C/h), Loading 1 (10 N); ASTM D1525 |
Entec Hyrene® PSCRY 2.5 General Purpose Polystyrene Available in North America Features: Crystal, General Purpose, and High Heat ResistanceRoHS Compliant Form: Pellets Information provided by Entec |
|||
Vicat Softening Point | 107 °C | 225 °F | |
Dow Retain® ABS 7490 ABS Data provided by Dow Chemical. |
|||
Vicat Softening Point | 107 °C @Load 1.00 kg, Thickness 3.17 mm |
225 °F @Load 2.20 lb, Thickness 0.125 in |
ASTM D1525 |
Diamond Polymers ASAPC TA-45 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Vicat Softening Point | 107 °C @Load 0.999 kg |
225 °F @Load 2.20 lb |
ISO 306 |
Arkema Group OREVAC® 18350P Grafted Maleic Anhydride Polyethylene OREVAC 18350P is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE and HDPE coating for steel pipeline. It is mainly used in pipe coating to have good adhesion pe.. |
|||
Vicat Softening Point | 107 °C | 225 °F | ASTM D1525 |
Americas Styrenics MB3150 High Heat Crystal Polystyrene Product CharacteristicsFast cycling due to high heat distortion temperatureHigh vicat softening temperatureExcellent clarity with slight blue tintGood toughnessFood Contact CompliantUL Classificatio.. |
|||
Vicat Softening Point | 107 °C | 225 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron SE-22M ABS Sheet Extrusion Grade Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali |
|||
Vicat Softening Point | 107 °C | 225 °F | ASTM D1525 |
Dow PELLETHANE® 2355-55DE Polyurethane Elastomer, Polyester Polyadipate Based
(discontinued **) Description: PELLETHANE® 2355-55DE polyester polyadipate based polyurethane elastomer has excellent oil and chemical resistance. Applications include: Film, Sheet, Tubing, Recreation and sporting e.. |
|||
Vicat Softening Point | 107 °C | 225 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CP8320 PC+ABS (Asia Pacific) Cycoloy Medium Heat Plating Grade for Automotive |