Lubrizol ESTANE® 5713 Ester Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 5713 Ester Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: It has the highest heat resistance of any Estane TPU resin used in adhesives. Supplied as pale amber granules, it is soluble in THF or THF/MEK blends. Higher heat resistance, tensile and bond strengths can be achieved with the addition of diisocyanates, peroxides, epoxies, and polyfunctional amides.Uses: Hot melt adhesive, solution cast films for lamination on fabricsAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Viscosity 130000 cP

@Temperature 204 °C
130000 cP

@Temperature 399 °F
ASTM D-1084-88
Brookfield Viscosity 800 - 1300 cP
800 - 1300 cP
RVT Spindle #2, 20 RPM, 23°C, 15% T.S. in THF
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
ASTM D2240
Tensile Strength 37.9 MPa
5500 psi
ASTM D412/D638
Elongation at Break 600 %
600 %
ASTM D412/D638
100% Modulus 0.00470 GPa
0.682 ksi
ASTM D412/D638
300% Modulus 0.00900 GPa
1.31 ksi
ASTM D412/D638
Peel Strength 0.400 kN/m
2.28 pli
ASTM D-1876-72
5.30 kN/m
30.2 pli
ASTM D-1876-72
7.20 kN/m
41.1 pli
TP-141
Thermal Properties Metric English Comments
Vicat Softening Point 95.0 °C
203 °F
ASTM D-1525
Glass Transition Temp, Tg -43.0 °C
-45.4 °F
DSC
Ring & Ball Softening Point 170 °C
338 °F
ASTM E-28-92
Descriptive Properties Value Comments
Gradient Bar Tack Temperature 84°C
Open Time >315 sex
ASTM D-4497-94