Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Estane® 58437 Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® 58437 Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® 58437 is an 85A aromatic polyester-based thermoplastic polyurethane (TPU).Features: Excellent cold temperature properties and improved heat resistance.Uses: Blown and flat die/cast film extrusion and tubing and profile extrusion.Information Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore A 82 - 88

@Time 5.00 sec
82 - 88

@Time 0.00139 hour
ASTM D2240
Tensile Strength 42.7 MPa
6190 psi
ASTM D412
Elongation at Break 560 %
560 %
ASTM D412
100% Modulus 0.00550 GPa
0.798 ksi
ASTM D412
300% Modulus 0.00970 GPa
1.41 ksi
ASTM D412
Tear Strength 24.5 kN/m
140 pli
Trouser; ASTM D470
Graves Tear Strength 78.9 kN/m
450 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 23

@Load 1.00 kg
23

@Load 2.20 lb
H-18 wheel; ASTM D3389
Tensile Set 12 %
12 %
200% elongation; ASTM D412
Thermal Properties Metric English Comments
Melting Point 167 °C
333 °F
DSC
168 °C
334 °F
Kofler
Glass Transition Temp, Tg -40.0 °C
-40.0 °F
DSC
Optical Properties Metric English Comments
Haze 5.4 %
5.4 %
pressed between glass; ASTM D1003
Processing Properties Metric English Comments
Zone 1 182 °C
360 °F
Extrusion
Zone 2 188 °C
370 °F
Extrusion
Zone 3 193 °C
379 °F
Extrusion
Zone 4 199 °C
390 °F
Extrusion
Adapter Temperature 199 °C
390 °F
5, Extrusion
Die Temperature 199 °C
390 °F
Zone 1, 6, Extrusion
199 °C
390 °F
Zone 2, Extrusion
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F
Descriptive Properties Value Comments
Volume Swell in Jet fuel (JP8) 4.9%
24h/23°C, ASTM D471
Users viewing this material also viewed the following: