Mechanical Properties Metric English Comments
300% Modulus 0.00970 GPa
1.41 ksi
ASTM D412
Network Polymers Softflex® 7700
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
300% Modulus 0.00970 GPa
1.41 ksi
ASTM D412
Network Polymers Softflex® 8910
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
300% Modulus 0.00970 GPa
1.41 ksi
Dow Pellethane® 2351-85AE Polyurethane Elastomer, Ether Based  (discontinued **)
PELLETHANE® 2351-85AE elastomer is a polyether hybrid specialty polyurethane elastomer compound which combines excellent resistance to fuels and oils with good hydrolytic stability and high damping..
300% Modulus 0.00970 GPa
1.41 ksi
ASTM D412
UBE UBEPOL BR340L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
300% Modulus 0.00970 GPa
1.41 ksi
DIN 53504
Lubrizol ESTANE® 58888 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
300% Modulus 0.00970 GPa
1.41 ksi
ASTM D412
UBE UBEPOL BR150B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
300% Modulus 0.00970 GPa
1.41 ksi
ASTM D412
Lubrizol Estane® 2102-75A Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Memory, elasticity and impact modificationAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane prod..
300% Modulus 0.00970 GPa
1.41 ksi
ASTM D412
Lubrizol ESTANE® 58271 Ester Based Thermoplastic Polyurethane
Features: Good physical properties, chemical resistance and adhesive properties and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding.Avai..
300% Modulus 0.00970 GPa
1.41 ksi
ASTM D412
Lubrizol ESTANE® 58325 Ether Based Thermoplastic Polyurethane
Features: High melt strength for thick sheet extrusion.Uses: Blown and Flat Die/Cast Extrusion, Tubing and Profile ExtrusionAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformat..
300% Modulus 0.00970 GPa
1.41 ksi
ASTM D412
Lubrizol Estane® 58437 Thermoplastic Polyurethane
Type: Estane® 58437 is an 85A aromatic polyester-based thermoplastic polyurethane (TPU).Features: Excellent cold temperature properties and improved heat resistance.Uses: Blown and flat die/cast fi..