Material Notes:
Type: Estane® ALR E65D is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ASTM D2240
Tensile Strength, Ultimate 57.2 MPa
8300 psi
ASTM D412
Elongation at Break 350 %
350 %
ASTM D412
100% Modulus 0.0179 GPa
2.60 ksi
ASTM D412
200% Modulus 0.0255 GPa
3.70 ksi
ASTM D412
300% Modulus 0.0434 GPa
6.30 ksi
ASTM D412
Flexural Modulus 0.317 GPa
46.0 ksi
ASTM D790