Lubrizol Estane® R198A-8 Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® R198A-8 Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® R198A-8 is a Shore 98A, polyether type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 98
98
ASTM D2240
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength, Ultimate 43.1 MPa
6260 psi
ASTM D412
Tensile Strength, Yield 14.7 MPa
2130 psi
at 100% elongation; ASTM D412
25.5 MPa
3700 psi
at 300% elongation; ASTM D412
Elongation at Break 545 %
545 %
ASTM D412
Tear Strength 132 kN/m
756 pli
Die C; ASTM D624
Compression Set 20 %

@Temperature 23.0 °C,
Time 79200 sec
20 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
45 %

@Temperature 70.0 °C,
Time 79200 sec
45 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395
Thermal Properties Metric English Comments
Vicat Softening Point 130 °C
266 °F
ASTM D1525