Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 132 kN/m | 753 pli | with incision; ISO 34B |
Lubrizol ESTANE® GP52DB Ester Based Thermoplastic Polyurethane Type: Estane® GP 52DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Tear Strength | 132 kN/m | 756 pli | Die C; ASTM D624 |
Lubrizol Estane® R198A-8 Thermoplastic Polyurethane Type: Estane® R198A-8 is a Shore 98A, polyether type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Information Provided by The Lubri.. |
|||
Tear Strength | 132 kN/m | 753 pli | Unnicked; ISO 34-1B |
Lubrizol Estane® GP 52 DT Thermoplastic Polyurethane Type: Estane® GP 52DT is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in E.. |