Lubrizol Estane® UB400 Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® UB400 Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® UB400 is a Shore 78A, polyester based, hot melt adhesive with excellent low temperature flexibility thermoplastic polyurethane (TPU).Uses: Extrusion, Powder Coating.Available in AsiaInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 200 °C
10 g/10 min

@Load 4.76 lb,
Temperature 392 °F
ASTM D1238
85 g/10 min

@Load 2.16 kg,
Temperature 220 °C
85 g/10 min

@Load 4.76 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
ASTM D2240
Thermal Properties Metric English Comments
Melting Point 107 °C
225 °F
Kofler; SRTM 3022-9
Glass Transition Temp, Tg -18.0 °C
-0.400 °F
ASTM D3418
Descriptive Properties Value Comments
Appearance Translucent
Flexibility (Hand) Soft