Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 85 g/10 min @Load 5.00 kg, Temperature 265 °C |
85 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® VX5011 PBT (Europe-Africa-Middle East) VALOX VX5011 is a 10% glass fibre reinforced PBT+PC blend with low warpage characteristics. |
|||
Melt Flow | 85 g/10 min @Load 5.00 kg, Temperature 266 °C |
85 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® VX5011 PBT (Europe-Africa-Middle East) VALOX VX5011 is a 10% glass fibre reinforced PBT+PC blend with low warpage characteristics. |
|||
Melt Flow | 85 g/10 min @Load 2.16 kg, Temperature 220 °C |
85 g/10 min @Load 4.76 lb, Temperature 428 °F |
ASTM D1238 |
Lubrizol Estane® UB400 Thermoplastic Polyurethane Type: Estane® UB400 is a Shore 78A, polyester based, hot melt adhesive with excellent low temperature flexibility thermoplastic polyurethane (TPU).Uses: Extrusion, Powder Coating.Available in AsiaI.. |