Lubrizol Stat-Rite® S-250 Static Control Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Lubrizol (former Noveon)
Trade Name Stat-Rite®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Stat-Rite® S-250 Static Control Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stat-Rite® S-250 is a static dissipative Polypropylene alloy. Stat-Rite S-250 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. Stat-Rite IDP alloys provide consistent static dissipation even when extruded, injection molded, or thermoformed into components. Features:Permanently static dissipativeHumidity insensitiveUltra-Clean: low off-gassing, low ionic contaminationColorableDurable: Can be used repeatedly.Applications:Semiconductor handlingMedical device packagingElectronic component handlingDisk packagingCleanroom suppliesAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
ASTM D792
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Tensile Modulus 1.28 GPa
185 ksi
ASTM D638
Flexural Modulus 1.28 GPa
185 ksi
ASTM D790-90
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256-92
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °C
163 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+10 ohm-cm
3.00e+10 ohm-cm
50% RH; ASTM D257
Surface Resistance 8.00e+8 ohm
8.00e+8 ohm
ESD S11.11; 12 % R.H.
Surface Resistivity per Square 8.00e+9 ohm
8.00e+9 ohm
50% RH; ASTM D257
Static Decay 0.010 sec
0.010 sec
FTMS-101C; 12% R.H., (+5000 V to 50 V)
0.010 sec
0.010 sec
FTMS-101C; 12% R.H., (-5000 V to -50 V)
0.50 sec
0.50 sec
Charged Plate Monitor; 50% R.H.
Tribocharge 10 V
10 V
Nitrile Glove - BFG Test Method
Descriptive Properties Value Comments
Color Light Blue