Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucas-Milhaupt Silvacore® A50N Flux Cored Brazing Alloy

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Lucas-Milhaupt
Trade Name Silvacore®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucas-Milhaupt Silvacore® A50N Flux Cored Brazing Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silvacote A50N Flux Coated Rod is a cadmium free silver brazing alloy that has found numerous applications for joining 300 series stainless steel in food, medical, and dental fields. Addition of nickel to the silver-copper zinc alloy imparts corrosion properties which retards joint or interface corrosion of the brazed assembly. The nickel element in Silvacote A50N also improves the bond strength when joining the tungsten carbide cutting tips. Typical applications are the joining of 300 series stainless steels in the food, medical, and dental fields.Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).
Physical Properties Metric English Comments
Specific Gravity 8.98 g/cc
8.98 g/cc
Density 8.98 g/cc
0.324 lb/in³
Thermal Properties Metric English Comments
Melting Point 660 - 707.2 °C
1220 - 1305 °F
Solidus 660 °C
1220 °F
Liquidus 707.2 °C
1305 °F
Maximum Service Temperature, Air 371 °C
700 °F
Component Elements Properties Metric English Comments
Boron, B 1.0 %
1.0 %
Metal (excluding flux)
Copper, Cu 19 - 21 %
19 - 21 %
Metal (excluding flux)
Nickel, Ni 1.5 - 2.5 %
1.5 - 2.5 %
Metal (excluding flux)
Other, total <= 0.15 %
<= 0.15 %
Metal (excluding flux)
Silver, Ag 49 - 51 %
49 - 51 %
Metal (excluding flux)
Zinc, Zn 27 - 29 %
27 - 29 %
Metal (excluding flux)
Electrical Properties Metric English Comments
Electrical Resistivity 0.00001175 ohm-cm
0.00001175 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 710 - 843 °C
1310 - 1550 °F
Brazing Temperature
Descriptive Properties Value Comments
Boric Acid % 27
percentage of flux
Color Light Yellow
Electrical Conductivity (% IACS) 15
Potassium Bifluoride % 26
percentage of flux
Potassium Fluoroborate % 25
percentage of flux
Potassium Tetraborate % 21
percentage of flux
Users viewing this material also viewed the following: