Material Notes:
Silvaloy 45 FC is the lowest melting brazing alloy available composed of silver, copper, zinc, and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joining steel, stainless steel, copper, copper alloys, nickel, nickel alloys or combinations of these metals. It has a wide acceptance by industrial users, as well as being included in Federal military specifications on brazing filler metals or alloys. It has a narrow melting range which is not apparent in most brazing operations, making it flow freely though a capillary. Typical applications are the joining of ferrous, non-ferrous, and dissimilar metals and alloys with close joint clearances.Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).
Physical Properties Metric English Comments
Specific Gravity 9.34 g/cc
9.34 g/cc
Density 9.41 g/cc
0.340 lb/in³
Thermal Properties Metric English Comments
Melting Point 607.2 - 618.3 °C
1125 - 1145 °F
Solidus 607.2 °C
1125 °F
Liquidus 618.3 °C
1145 °F
Component Elements Properties Metric English Comments
Cadmium, Cd 13.93 - 15.93 %
13.93 - 15.93 %
Copper, Cu 4.33 - 14.33 %
4.33 - 14.33 %
As balance of metal
Silver, Ag 27 - 29 %
27 - 29 %
Zinc, Zn 7.96 - 11.96 %
7.96 - 11.96 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000606 ohm-cm
0.00000606 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 618.3 - 760 °C
1145 - 1400 °F
Brazing Temperature
Descriptive Properties Value Comments
Boric Acid % 0-30
percentage of flux
Color Light Yellow
Colored Pigments % 0-0.05
percentage of flux
Electrical Conductivity (% IACS) 27.6
Flux 36.78-38.78%
Potassium Bifluoride % 0-30
percentage of flux
Potassium Fluoroborate % 0-30
percentage of flux
Potassium Pentaborate % 1-5.0
percentage of flux
Potassium Tetraborate % 0-40
percentage of flux
Sodium Dodecyl Sulfate % 0-0.5
percentage of flux