Lucent Polymers G66-33 Nylon 66, 33% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Lucent Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucent Polymers G66-33 Nylon 66, 33% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Add "H" for Heat Stabilized Add "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 cm/cm

@Thickness 3.17 mm
0.0040 in/in

@Thickness 0.125 in
1/8" Section
Mechanical Properties Metric English Comments
Tensile Strength, Yield 137.93 MPa
20005 psi
ASTM D638
Elongation at Break >= 3.0 %
>= 3.0 %
ASTM D638
Flexural Strength 220.69 MPa
32008 psi
ASTM D790
Flexural Modulus 7.586 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
1.20 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 250 - 265 °C
482 - 509 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 243.33 °C
469.99 °F
ASTM D648