Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 250 °C | 482 °F | STN EN 11357-1 |
Plastcom SLOVASTER® B1 GF 15 FRL 4 PBT reinforced with glass fibers, flame retarded PBT reinforced with 15 % glass fiber, flame retarded with the halogen flame retardant. Anisotropy of shrinkage enables the injection molding of round, cylindrical or other hole products. Application.. |
|||
Melting Point | 250 - 258 °C | 482 - 496 °F | DSC @ 15°C / min; ASTM D3418 |
Ovation Polymers RIGITRON 30530 GF Polyester, 30% Glass Reinforced Polyester – 30 % Glass Fiber Reinforced PET. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Va.. |
|||
Melting Point | 250 - 258 °C | 482 - 496 °F | DSC @ 15°C / min; ASTM D3418 |
Ovation Polymers RIGITRON 30545 GF Polyester, 45% Glass Reinforced Polyester – 45% Glass Fiber Reinforced PET. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Var.. |
|||
Melting Point | 250 - 256 °C | 482 - 493 °F | QCD--W1-49 |
Pearl Engineering PEPLPET FR-101-H Monofilament Resin Used as textile grade flame retardant for furniture, car and plane upholstery. |
|||
Melting Point | 250 °C | 482 °F | Crystalline Peak Melting Point; ASTM D3418 |
Eastman 9663 PET
(discontinued **) VORIDIAN PET 9663 is a PET homopolymer widely used in the heatset industry and is FDA approved for food contact in hotfill applications. Voridian PET 9663 has a wide processing window and it’s vers.. |
|||
Melting Point | 250 - 272 °C | 482 - 522 °F | |
Indium Corp. Indalloy 259 Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 250 - 256 °C | 482 - 493 °F | |
Tisan TISAPET® 30% Glass Reinforced Polyethylene Terephthalate Properties:Excellent mechanical propertiesHigh thermal-chemical friction resistanceGood electrical propertiesGood rate of melt flow index relative to the quantity of glass fiberBalanced electrical a.. |
|||
Melting Point | 250 °C | 482 °F | ISO 3146 |
Wellman Wellpet® GF100-BK1 PET, 30% Glass Fiber Reinforced Typical data obtained from injection molded test bars, tested dry as molded at 73°F (23°C). Information provided by Wellman, Inc. Engineering Resins Division. |
|||
Melting Point | 250 °C | 482 °F | DSC |
Wolf Kunststoff ZEDEX® ZX-100K A1K Polymer Alloy Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good weather resistance; Good machinability; FDA compliant LABS; PTFE and silicone-free; KTW approved; Stress resistantApplications: .. |
|||
Melting Point | 250 °C | 482 °F | 10°C/min; ISO 11357-1/-3 |
DSM EcoPaXX® Q-KG6 PA410-GF30 % Glass Reinforced, Heat Stabilized, for E&E applications |
|||
Melting Point | 250 - 260 °C | 482 - 500 °F | |
Daikin NEOFLON NP-130 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Heavy wall wire insulation, cable jacketing, pipe, shrinka.. |
|||
Melting Point | <= 250 °C | <= 482 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 1001X26 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Melting Point | <= 250 °C | <= 482 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 1001X74 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Melting Point | <= 250 °C | <= 482 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 1004YB Film Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 1004YB is an LLDPE grade, offering excellent high temperature stability. Properties may be further enhanced by the combination with Exceed mLLDPE. Availability: Africa & Midd.. |
|||
Melting Point | 250 °C | 482 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Rynite® 515CS BK575M PET Rynite® 515CS BK575M is a 15% glass fiber reinforced, black polyethylene terephthalate resin modified for improved color stability after heat aging.Information provided by DuPont Performance Polyme.. |
|||
Melting Point | 250 °C | 482 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® 84G33 BKB031 Nylon 66 + Nylon 6
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 + Polyamide 6 Zytel 84G33 BKB031 is a 33% glass reinforced toughened polyamide 66 and polyamide 6 co-melt black cube blended resin. This resin was develop.. |
|||
Melting Point | 250 °C | 482 °F | 10°C/min; ISO 11357-1/-3 |
DSM EcoPaXX® Q150-D PA410 Low/Medium Viscosity |
|||
Melting Point | 250 °C | 482 °F | 10°C/min; ISO 11357-1/-3 |
DSM EcoPaXX® Q-HG10 PA410-GF50 50% Glass Reinforced, Heat Stabilized |
|||
Melting Point | 250 °C | 482 °F | 10°C/min; ISO 11357-1/-3 |
DSM EcoPaXX® Q-KGS6 PA410-GF30 FR 30% Glass Reinforced, Flame Retardant (Halogen free) |
|||
Melting Point | 250 °C | 482 °F | 10°C/min; ISO 11357-1/-3 |
DSM EcoPaXX® Q-X07290 PA410-I Impact Modified |
|||
Melting Point | 250 °C | 482 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Rynite® 408 BK515 PET Rynite® 408 BK515 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness and temperature resistance.Info.. |
|||
Melting Point | 250 °C | 482 °F | [10 K/min], ISO 11357 |
Eurotec® Tecopet® PT74 CR20 BK111 PR PET, 20% carbon fiber reinforced, black, fast crystallization grade Information provided by Eurotec® |
|||
Melting Point | 250 °C | 482 °F | [10 K/min], ISO 11357 |
Eurotec® Tecopet® PT74 GR30 BK002 DA PET, 30% glass fiber reinforced, high heat stabilized, black Information provided by Eurotec® |
|||
Melting Point | 250 °C | 482 °F | ISO 11357-3 |
Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, DAM Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters.. |