Material Notes:
UV Stable/Weatherable, f1 RatedMelt Flow Adjustable for Application UL File Number: E213588Information provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0060 cm/cm

@Thickness 3.17 mm
0.0060 in/in

@Thickness 0.125 in
1/8" Section
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.07 MPa
9003 psi
ASTM D638
Elongation at Break >= 130 %
>= 130 %
ASTM D638
Flexural Strength 90.34 MPa
13100 psi
ASTM D790
Flexural Modulus 2.276 GPa
330.1 ksi
ASTM D790
Izod Impact, Notched 6.41 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
12.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 132.22 °C
270.00 °F
ASTM D648
UL RTI, Mechanical without Impact 105 °C
221 °F
Flammability, UL94 V-0
V-0
5VA
5VA