Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 132.22 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 132.22 °C
270.00 °F
ASTM D648
Lucent Polymers PC-1403 Polycarbonate, Extrusion/Blow Molding Grade
Medium FlowAdd "R" for Added ReleaseAdd "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 132.22 °C
270.00 °F
ASTM D648
Lucent Polymers PC-1403FD Polycarbonate, FDA Compliant, Extrusion/Blow Molding Grade
Medium FlowAdd "R" for Added ReleaseAdd "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 132.22 °C
270.00 °F
ASTM D648
Lucent Polymers PC-1406 Polycarbonate, Extrusion/Blow Molding Grade
Medium FlowAdd "R" for Added ReleaseAdd "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 132.22 °C
270.00 °F
ASTM D648
Lucent Polymers PC-1406FD Polycarbonate, FDA Compliant, Extrusion/Blow Molding Grade
Medium FlowAdd "R" for Added ReleaseAdd "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 132.22 °C
270.00 °F
ASTM D648
Lucent Polymers PC-1410 Polycarbonate, Injection/Extrusion Grade
Medium FlowAdd "R" for Added ReleaseAdd "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 132.22 °C
270.00 °F
ASTM D648
Lucent Polymers PC-1410FD Polycarbonate, FDA Compliant, Injection/Extrusion Grade
Medium FlowAdd "R" for Added ReleaseAdd "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 132.22 °C
270.00 °F
ASTM D648
Lucent Polymers PC-1418 Polycarbonate, Injection Grade
High FlowAdd "R" for Added ReleaseAdd "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 132.22 °C
270.00 °F
ASTM D648
Lucent Polymers PC-1418FD Polycarbonate, FDA Compliant, Injection Grade
High FlowAdd "R" for Added ReleaseAdd "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 132.22 °C
270.00 °F
ASTM D648
Lucent Polymers PC-1425 Polycarbonate, Injection Grade
High FlowAdd "R" for Added ReleaseAdd "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 132.22 °C
270.00 °F
ASTM D648
Lucent Polymers PC-1428 Polycarbonate, Injection Grade
High FlowAdd "R" for Added ReleaseAdd "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 132.22 °C
270.00 °F
ASTM D648
Lucent Polymers PC-1428FD Polycarbonate, FDA Compliant, Injection Grade
High FlowAdd "R" for Added ReleaseAdd "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 132.22 °C
270.00 °F
ASTM D648
Lucent Polymers PC-FR0 Polycarbonate, Flame Resistant
UV Stable/Weatherable, f1 RatedMelt Flow Adjustable for Application UL File Number: E213588Information provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 132.22 °C
270.00 °F
ASTM D648
Lucent Polymers PC-FR2 Polycarbonate, Flame Resistant
Melt Flow Adjustable for ApplicationUL File Number: E213588Add "R" for Added ReleaseAdd "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 132.22 °C
270.00 °F
ASTM D648
Lucent Polymers POM-100 Acetal Copolymer, General Purpose, Injection Grade
Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 132.22 °C
270.00 °F
ASTM D648
Lucent Polymers POM-270 Acetal Copolymer, Easy Flow, Injection Grade
Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.