Lucent Polymers PC/ABS-1020 Polycarbonate+ABS, General Purpose, Injection Grade

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Lucent Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucent Polymers PC/ABS-1020 Polycarbonate+ABS, General Purpose, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0060 cm/cm

@Thickness 3.17 mm
0.0060 in/in

@Thickness 0.125 in
1/8" Section
Melt Flow 20 g/10 min

@Load 5.00 kg,
Temperature 260 °C
20 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 56.55 MPa
8202 psi
ASTM D638
Elongation at Break >= 140 %
>= 140 %
ASTM D638
Flexural Strength 86.21 MPa
12500 psi
ASTM D790
Flexural Modulus 2.317 GPa
336.1 ksi
ASTM D790
Izod Impact, Notched 5.34 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
10.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 112.78 °C
235.00 °F
ASTM D648