Material Notes:
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.01 cm/cm

@Thickness 3.17 mm
0.01 in/in

@Thickness 0.125 in
1/8" Section
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Elongation at Break >= 25 %
>= 25 %
ASTM D638
Flexural Strength 30.0 MPa
4350 psi
ASTM D790
Flexural Modulus 0.862 GPa
125 ksi
ASTM D790
Izod Impact, Notched 9.99 J/cm

@Thickness 3.17 mm
18.7 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 43.0 °C
109 °F
ASTM D648
Users viewing this material also viewed the following: