Lucite International Elvacite ® 2927 Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Elvacite ®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Elvacite ® 2927 Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lucite International has developed novel polymer chemistry which delivers Elvacite® thermoplastic acrylic resins with controlled molecular architecture and enables the coatings formulator to achieve higher solids solutions / lower VOC emissions without significant compromise to physical properties or causing odor problems. The technology has been developed with a VOC limit target of 3.5 lb./gal.Elvacite® 2927 can be employed in a wide range of inks and coatings systems, where the increased solids or reduced solution viscosity are desired. Typical applications include: Industrial Coatings, Concrete Coatings, Marine Paints, Solvent based Inks, UV Coatings and Inks.Information provided by Lucite International
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
Viscosity Measurement 0.11 - 0.13
0.11 - 0.13
Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Molecular Weight 19000 g/mol
19000 g/mol
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 46.0 °C
115 °F
Chemical Properties Metric English Comments
Total Acid Number 3.5
3.5
Processing Properties Metric English Comments
Moisture Content 0.65 %
0.65 %