Lucite International Lucite® 41 Acrylic Bead Resin

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, General Purpose, Molded
Manufacturer Lucite International
Trade Name Lucite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Lucite® 41 Acrylic Bead Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lucite® 41 is used for casting and embedment and has a lower optical quality than other Lucite® grades. It is a methyl methacrylate homopolymer.General Lucite® Acrylic Bead Resin Information: Used in casting and embedment, compression molding, dental applications, or glass separation. End products have outstanding UV resistance, Excellent weatherability, superior abrasion resistance, excellent resistance to water, alcohol, dilute acids and bases, chemical fumes, and corrosive/oxidizing environments, high gloss and hardness, water-white color and transparency, and resistance to discoloration when heated. Lucite® resins are available as minute spherical beads, water-white only (no tints) and transparent. Thermally stable to 230°C. At higher temperatures (260°C and above), they undergo smooth depolymerization to monomers, leaving negligible ash.Data provided by the manufacture. Properties reported below are from test specimens machined from compression molded parts.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
Water Absorption 0.47 %
0.47 %
24h
Mechanical Properties Metric English Comments
Hardness, Rockwell M 81
81
Tensile Strength, Ultimate 55.0 MPa
7980 psi
Elongation at Break 1.0 %
1.0 %
23°C, 50% RH
Optical Properties Metric English Comments
Refractive Index 1.491
1.491
n<sub>D</sub>
Transmission, Visible 92 %
92 %
Luminous Transmission at 3.18 mm (0.125 in.)