Material Notes:
Lucite® acrylic resins are used in a variety of industrial, commercial and architectural applications. They’re a favorite among manufacturers of commemorative embedments because of their exceptional optical clarity and hardness. The widely-used technique of casting with a slurry mixture of Lucite® resin and methyl methacrylate monomer produces fine embedments suitable for use as service awards, sales aids, anniversary commemorations, and product displays.Lucite® 6751 is the highest quality resin for embedment work because of it’s small average particle size distribution and enhanced optical clarity.Information provided by Lucite International
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0431 lb/in³
Water Absorption 0.47 %
0.47 %
Particle Size 75 - 105 µm
75 - 105 µm
Viscosity Measurement 1.2
1.2
Inherent viscosity
Mechanical Properties Metric English Comments
Hardness, Rockwell M 81
81
Tensile Strength 53.8 MPa
7800 psi
Elongation at Break 1.0 %
1.0 %
Optical Properties Metric English Comments
Transmission, Visible 92 %
92 %