Lucite International Perspexâ„¢ GS IM Acrylic Cast Sheet OM14

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Cast
Manufacturer Lucite International
Trade Name Perspex™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Perspexâ„¢ GS IM Acrylic Cast Sheet OM14.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PERSPEX cast sheet is made between sheets of high quality glass and produced in batches. It has a very high molecular weight making it strong, resilient and easy to handle and fabricate. The cast method of manufacture is ideally suited to small colour runs and batch sizes. Information provided by Lucite International.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Rockwell M 98.5
98.5
ISO 2039-2
Tensile Strength, Ultimate 62.0 MPa
8990 psi
5 mm/min; ISO 527
Flexural Strength 105 MPa
15200 psi
2 mm/min; ISO 178
Flexural Modulus 2.96 GPa
429 ksi
2 mm/min; ISO 178
Charpy Impact Unnotched 2.17 J/cm²
10.3 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.120 J/cm²
0.571 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Vicat Softening Point >= 110 °C
>= 230 °F
ISO 306A
Flammability, UL94 HB
HB
Flammability Test 3.0
3.0
BS 476, Pt7