LyondellBasell Pro-fax 6301 Polypropylene Homopolymer, Flake Resin

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Pro-fax
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Pro-fax 6301 Polypropylene Homopolymer, Flake Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Primary Processing Method: Masterbatch/ConcentratesKey Features: general purpose polypropylene homopolymer flake resin, minimal stabilization, FDA acceptableApplications: compounding, concentrates, masterbatchesMeets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications. Additives require a reassessment.Description: Pro-fax 6301 general purpose polypropylene homopolymer resin is available as natural flake. Flake from resin is well suited fro mixing with pigments and other additives to make polymer concentrates or masterbatches. This resin has very minimal stabilization, which allows wide design latitude for the compounded. Additional suitable stabilization is required to protect the resin during melt processing and throughout its useful life. Pro-fax 6301 flake resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. Please note that any additives compounded into this resin will require a reassessment of its FDA status. All ingredients meet the chemical registration requirements of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792B
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785A
Tensile Strength, Yield 34.0 MPa
4930 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.40 GPa
203 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.360 J/cm
0.674 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
ASTM D648