Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | >= 1.40 GPa | >= 203 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 1500N (F30G) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Flexural Modulus | >= 1.40 GPa | >= 203 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 1525J (T28F) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | at 1% Secant; ASTM D790 |
NOVA Chemicals Novapol® HB-W555-AC PE Blow Molding Resin High molecular weight, High rigidity, Excellent impact strength, Excellent ESCR, Used in high purity chemical packagingInformation provided by NOVA Chemicals. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ASTM D 790 |
NOVA Chemicals Novapol® HB-W555-EC HDPE Blow Molding Resin HB-W555-EC complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biolo.. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ISO 178 |
SABIC Innovative Plastics LNP Faradex MS002P PP (Europe-Africa-Middle East) LNP* Faradex* MS002P is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Exceptional Processi.. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ISO 178 |
Solvay Engineered Polymers SEQUEL® 2325 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 2325 engineered polyolefin is designed for mold-in-color automotive interior applications. This material exhibits excellent low-gloss surface appearance and processability. Ap.. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Pro-fax 6301 Polypropylene Homopolymer, Flake Resin Primary Processing Method: Masterbatch/ConcentratesKey Features: general purpose polypropylene homopolymer flake resin, minimal stabilization, FDA acceptableApplications: compounding, concentrates, .. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | DIN 53457 |
Schwartz Technical Plastics LAMIGAMID® 100 Polyamide 6, Extruded, Conditioned Application: machine parts under 80 mm diameter, hammer-heads, cup-shaped bearing shellsInformation provided by Schwartz Technical Plastics GmbH |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | |
SPS Guang Zhou SAMATâ„¢ 168(f1) Flame-retarded Polypropylene Characteristic: Good flame resistance, good chemical resistance, good mechanical propertiesApplications: X'mas decorative product, E/E applianceInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | 5 mm/min; GOST 9550 |
Sibur H250 GP Polypropylene Homopolymer Polypropylene homopolymer with narrow molecular weight distribution. It features high fluidity, an optimal stabilization package and balanced physical and mechanical properties.general purpose produ.. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | 1mm/min; ISO 178 |
Borealis BS2581 High Density Polyethylene for Blow Molding BS2581 is a high density polyethylene intended for blow molding products with high stiffness and very good environmental stress crack resistance (ESCR). Applications: industrial chemicals, househol.. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ASTM D790 |
A. Schulman POLYFORT™ FXP 1227U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1227U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ASTM-D790 |
Polyram RamLloy PVB101 ABS/NYLON alloy, Impact Modified Impact modified ABS/NYLON alloy for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | tangent; ASTM D790 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ISO 527-2 |
Total PPC 7650 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 7650 is a nucleated and antistatic heterophasic copolymer. PPC 7642 is characterized by a medium fluidity offering a combination of ease of processing and excellent impact propert.. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | tangent; ASTM D790 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | tangent; ASTM D790 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ASTM D 790 |
Cossa Polimeri ESTAPROP 1000 V2 H Flame Retardant Polypropylene PP homopolymerFlame retardant class V2, PBDE free, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | 2 mm/min, 4 mm; ISO 178 |
Chi Mei Kibiton® PB-5903 SBC High transparency, high toughness, PS Impact modifier |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ISO 178 |
Eurostar Staramide R1000IX4 PA66, Impact Modified, Injection Molded Staramide R1000IX4 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI020 Star X 1020)Information provided by Eurostar. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0437C40L1 Calcium Reinforced |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0437T20L Talc Reinforced |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0436C30L Calcium Reinforced |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ASTM D790 |
Buckeye Polymers BP RPP 1012 C Polypropylene, 10% Mineral Filled Calcium carbonate-filled PP grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. This material can be customized through the addition of UV packag.. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ISO 178 |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Conditioned) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ASTM D790 |
Teknor Apex Sinelec CCB6814 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Electrically Conductive Uses: Corrugated Sheet Forms: Pellets Processing Method: Injection Method; Sheet Extr.. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ISO 178 |
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Conditioned) Ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase.. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ASTM D790 |
Braskem H 152 Fiber Extrusion Polypropylene Applications: Nonwoven by blow process for disposable diapers, personal care and disposable medical care. Information provided by Braskem |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | 1% secant; ASTM D790 |
Braskem H 401 Cast Film Extrusion Polypropylene Description: H 401 is a medium melt flow rate homopolymer polypropylene, additived with slip and antiblocking agents. Designed specially for cast film. This product features good impact strength, ex.. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | Tangent at 0.05 in/min; ASTM D790A |
LyondellBasell Astryn 6652 Polypropylene Homopolymer Key Features: low melt flow, medium modulus polypropylene homopolymer, high strength, high impact, good hydrolytic abilityApplications: water pipe fittings and connectorsDescription: Astryn 6652 low.. |