LyondellBasell Pro-fax 6331W Polypropylene Homopolymer, Antistat

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Pro-fax
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Pro-fax 6331W Polypropylene Homopolymer, Antistat.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: antistatic polypropylene homopolymer resin, FDA acceptable, resists dust pickup, low odor transferApplications: containers, closures, hospital and institutional ware, toysMeets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.Description: Pro-fax 6331W easy molding polypropylene homopolymer resin features antistatic properties. This resin is available in pellet form. It meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. This resin has a UL yellow card RTI, which applies to all colors. All ingredients meet the chemical registration requirements of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792B
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 89
89
ASTM D785A
Tensile Strength, Yield 34.0 MPa
4930 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.50 GPa
218 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.340 J/cm
0.637 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C
198 °F
ASTM D648
UL RTI, Mechanical with Impact 65.0 °C
149 °F
Minimum thickness 0.038 inches.
Flammability, UL94 HB
HB
Minimum thickness 0.038 inches.
Users viewing this material also viewed the following: