Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Pro-fax SA861 Polypropylene Random Copolymer, Cast Film Extrusion

Category Polymer , Film , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Pro-fax
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Pro-fax SA861 Polypropylene Random Copolymer, Cast Film Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: polypropylene random copolymer resin formulated for cast film extrusion, good optical properties, excellent slip properties, FDA acceptable, improved cold temperature impact resistanceApplications: bags for hosiery, packaging for produce, sheet protectors, photograph pockets, card display sleevesMeets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.Description: Pro-fax SA861 polypropylene random copolymer resin, formulated with slip and antilock, is designed for cast film packaging applications. Cast film made with this resin has exceptional clarity and gloss, as well as improved cold temperature impact resistance and broader heat seal range compared to homopolymer polypropylene. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792B
Thickness 25.4 microns
1.00 mil
Melt Flow 6.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Film Elongation at Break, TD 710 %
710 %
ASTM D882A
Elongation at Yield 13 %
13 %
ASTM D638
Flexural Modulus 0.920 GPa
133 ksi
1% secant at 0.05 in/min; ASTM D790A
Secant Modulus, MD 0.655 GPa
95.0 ksi
Film; 1% secant; ASTM D882A
Secant Modulus, TD 0.621 GPa
90.1 ksi
1% secant; ASTM D882A
Izod Impact, Notched 0.560 J/cm
1.05 ft-lb/in
ASTM D256A
Coefficient of Friction 0.15 - 0.25
0.15 - 0.25
ASTM D1894
Elmendorf Tear Strength MD 25 g
25 g
ASTM D1922A
Elmendorf Tear Strength TD 500 g
500 g
ASTM D1922A
Elmendorf Tear Strength, MD 0.984 g/micron
25.0 g/mil
ASTM D1922A
Elmendorf Tear Strength, TD 19.7 g/micron
500 g/mil
ASTM D1922A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °C
169 °F
ASTM D648
Optical Properties Metric English Comments
Haze 3.0 %
3.0 %
ASTM D1003A
Gloss 80 - 85 %
80 - 85 %
at 45°; ASTM D2457
Users viewing this material also viewed the following: