Polymer Property : Secant Modulus, TD = 90.1 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.621 - 0.703 GPa
90.1 - 102 ksi
ASTM D882
Honeywell PMP Polymethylpentene Film  (discontinued **)
PMP is a clear, red, or blue film manufactured from polymethylpentene. It provides more toughness and heat resistance than standard polyolefins for release film applications.Information provided by..
Secant Modulus, TD 0.621 GPa
90.1 ksi
1% secant; ASTM D882A
LyondellBasell Pro-fax SA861 Polypropylene Random Copolymer, Cast Film Extrusion
Key Features: polypropylene random copolymer resin formulated for cast film extrusion, good optical properties, excellent slip properties, FDA acceptable, improved cold temperature impact resistance..