M. Holland Company CP510 Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer M. Holland Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company CP510 Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Additives: Heat Stabilizer, Nucleating AgentsFeatures: High Flow, High Impact Resistance, Heat Stabilizer, NucleatedUses: Construction Applications, Lawn and Garden EquipmentApprovals: FDA 21 CFR 177.1520 Processing Method: Injection MoldingInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 75
75
ASTM D785
Tensile Strength, Yield 21.7 MPa
3150 psi
ASTM D638
Flexural Modulus 1.07 GPa
155 ksi
ASTM D790
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
at 73°F; ASTM D256
Gardner Impact 24.8 J
18.3 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM D648
Descriptive Properties Value Comments
Form Pellets