Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 308.47 g/mol
308.47 g/mol
Descriptive Properties Value Comments
Assay 18% Cd
CAS Number 10022-68-1
Form White powder
Purity 99.999%
Typical Impurities Ca, Cu, Fe, Mg, Zn < 1 ppm