MV Labs GA1000 Ga2(SO4)3·xH2O Gallium sulfate hydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs GA1000 Ga2(SO4)3·xH2O Gallium sulfate hydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 427.62 g/mol
427.62 g/mol
Descriptive Properties Value Comments
Assay 36% Ga
CAS Number 13780-42-2
Form White crystals
Purity 99.999%
Typical Impurities Cd, Cr, Cu, In, Si, Zn < 1 ppm