Magyar Aluminum ALOLT 01 Aluminum Hydroxide

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Magyar Aluminium
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Magyar Aluminum ALOLT 01 Aluminum Hydroxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dry type
Physical Properties Metric English Comments
Bulk Density <= 1.40 g/cc
<= 0.0506 lb/in³
Brightness >= 75 %
>= 75 %
Whiteness
Particle Size 40 - 80 µm
40 - 80 µm
d50
Component Elements Properties Metric English Comments
Fe2O3 <= 0.020 %
<= 0.020 %
Na2O <= 0.20 %
<= 0.20 %
SiO2 <= 0.010 %
<= 0.010 %
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Aluminum Hydroxide (%) >99.5