Mallard Creek Polymers ROVENE® 40554 Vinyl Acrylic Emulsion

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Mallard Creek Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mallard Creek Polymers ROVENE® 40554 Vinyl Acrylic Emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ROVENE® 40554 is a medium soft, vinyl acrylic copolymer latex with good heat and light stability, and excellent mechanical stability.APPLICATIONS: ROVENE® 40554 is recommended for various nonwoven and paper saturation applications.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Solids Content 46 - 48 %
46 - 48 %
Particle Size 0.25 µm
0.25 µm
pH 4.5 - 5.5
4.5 - 5.5
Brookfield Viscosity <= 200 cP
<= 200 cP
#2/20 rpm
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -11.0 °C
12.2 °F
Descriptive Properties Value Comments
Emulsifiers Anionic
Residual Monomer 0.09% Max