Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 200 cP @Temperature 25.0 °C |
200 cP @Temperature 77.0 °F |
No. 3 Spindle, 100 rpm |
Omya HYDROCARB® 90 Calcium Carbonate An ultrafine ground calcium carbonate for paper and board coating.Information supplied by Omya North America. |
|||
Brookfield Viscosity | 200 cP @Temperature 25.0 °C |
200 cP @Temperature 77.0 °F |
No. 3 Spindle, 100 rpm |
Omya HYDROCARB® 90 HS Calcium Carbonate An ultrafine ground calcium carbonate for paper and board coating.Information supplied by Omya North America. |
|||
Brookfield Viscosity | 200 cP | 200 cP | dry |
Omya OMYACARB® F - FL Calcium Carbonate A high purity, ultrafine, wet ground natural calcium carbonate available in dry or slurry form.Applications: Plastic applications such as rigid PVC and flexible PVC. Paint applications such as water.. |
|||
Brookfield Viscosity | 200 cP @Temperature 25.0 °C |
200 cP @Temperature 77.0 °F |
No. 3 Spindle, 100 rpm |
Omya OMYAFIL® Calcium Carbonate An ultrafine ground calcium carbonate for paper and board filling.Information supplied by Omya North America. |
|||
Brookfield Viscosity | 200 cP | 200 cP | One Day Viscosity @ 30rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series 171 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 171 is an ultra-high molecular weight, fine particle size homopolymer dispersion resin intended for use in thin, organosol cast coatings and films. This resin provides excellent fused film an.. |
|||
Brookfield Viscosity | 200 cP | 200 cP | One Hour Viscosity @ 30rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series 178 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 178 is a high molecular weight, fine particle size homopolymer dispersion resin. It provides the ability to produce thin gauge coatings. It is recommended for applications such as food and be.. |
|||
Brookfield Viscosity | 200 cP | 200 cP | One Day Viscosity @ 30rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series 4195 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 171 is an ultra-high molecular weight, fine particle size homopolymer dispersion resin intended for use in thin, organosol cast coatings and films. This resin provides excellent fused film an.. |
|||
Brookfield Viscosity | 200 cP | 200 cP | One Hour Viscosity @ 30 rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series L100UF Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Ultrafine 170-L100UF is a medium molecular weight, ultrafine particle size homopolymer dispersion resin. With the very fine particle size, it provides excellent casting characteristics for th.. |
|||
Brookfield Viscosity | 200 cP | 200 cP | 20 rpm; ASTM D1417 |
Polimeri Europa Europrene Latice® 1251 Carboxylated Styrene - Butadiene Copolymer Europrene Latice® 1251 is an aqueous dispersion of a carboxylated styrene-butadiene copolymer obtained using synthetic anionic emulsifiers. It contains an antioxidant.Key Features: Europrene Lati.. |
|||
Brookfield Viscosity | 200 - 400 cP @Temperature 20.0 °C |
200 - 400 cP @Temperature 68.0 °F |
Brookfield RVF sp. 2, 20 rpm solution at 15% in MEK; MQSA N0 40A |
Lubrizol Advanced Materials Pearlstick® 45-50/03 Linear Thermoplastic Polyurethane Elastomer
(discontinued ** Pearlstick 45-50/03 is an elastic, linear, aromatic polyurethane with an extremely high crystallization rate and a medium-low thermoplasticity level, available as pellets.Solubility: Pearlstick 45-.. |
|||
Brookfield Viscosity | 200 - 400 cP @Temperature 20.0 °C |
200 - 400 cP @Temperature 68.0 °F |
Brookfield RVF sp. 3, 20 rpm solution at 15% in MEK; MQSA N° 40A |
Lubrizol Advanced Materials Pearlstick® 49-46/03 Linear Thermoplastic Polyurethane Elastomer
(discontinued ** Pearlstick 49-46/03 is an elastic, linear, aromatic polyurethane with a very high crystallization rate and a low thermoplasticity level, available as pellets.Solubility: Pearlstick 49-46/03 is solu.. |
|||
Brookfield Viscosity | 200 cP | 200 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4076 SBR Latex ROVENE® 4076 is a medium firm carboxylated styrene - butadiene emulsion designed for use in formulating high performance architectural coatings including flat wall paints and primer-sealers. When.. |
|||
Brookfield Viscosity | 200 - 700 cP | 200 - 700 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4151 SBR Latex ROVENE® 4151 is a carboxylated styrene-butadiene emulsion that has a soft, resilient hand with above average strength properties. It may be compounded with a wide variety of fillers and additives.. |
|||
Brookfield Viscosity | 200 - 1000 cP | 200 - 1000 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4170 SBR Latex ROVENE® 4170 is a carboxylated styrene-butadiene emulsion that has a medium-firm hand with outstanding strength properties. This binder is especially suited for various textile and coating applic.. |
|||
Brookfield Viscosity | 200 - 800 cP | 200 - 800 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4220 SBR Emulsion ROVENE® 4220 is a new developmental polymer specifically designed to be used flooring adhesives as well as an extender for chloroprene and natural latex in contact adhesives and other cohesive an.. |
|||
Brookfield Viscosity | <= 200 cP | <= 200 cP | Spindle # 2, rpm 60 |
Michelman® DigiGuard® Gloss 110 Overprint varnish Description: Overprint varnish for flexible packagingUsage: DigiGuard® Gloss 110 is a high gloss, temperature resistant, water based overprint varnish which meets FDA food contact requirements.Ap.. |
|||
Brookfield Viscosity | <= 200 cP | <= 200 cP | Spindle # 2, rpm 60 |
Michelman® Michem® Emulsion 41740 Nonionic, polyethylene emulsion Description: Nonionic, polyethylene emulsionUsage: Michem® Emulsion 41740 is used for release and water resistance in specialty coated films and papers. It is also an effective tactile modifier f.. |
|||
Brookfield Viscosity | <= 200 cP | <= 200 cP | Spindle # 2, rpm 60 |
Michelman® Michem® Emulsion 48040M2 Nonionic microcrystalline wax emulsion Description: Nonionic microcrystalline wax emulsionUsage: Michem® Emulsion 47950 is a wax emulsion which is effective as an anti-graffiti and sacrificial coating and can also contribute water res.. |
|||
Brookfield Viscosity | <= 200 cP | <= 200 cP | Spindle # 2, rpm 60 |
Michelman® Michem® Flex P1852 Water based primer Description: Water based primer for liquids and extrusion coated resins.Usage: Michem® Flex P1852 is a Primer for film, metal and paper substrates to promote adhesion to extrusion coated resins r.. |
|||
Brookfield Viscosity | 200 - 650 cP | 200 - 650 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Coat 40EAF Water resistant, gluable coating with good grease resistance Description: Water resistant, gluable coating with good grease resistanceUsage: Michem® Coat 40EAF is a versatile water resistant coating which demonstrates some grease resistance as well. It is .. |
|||
Brookfield Viscosity | 200 - 400 cP | 200 - 400 cP | Brookfield RVF sp 2, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A |
Lubrizol Advanced Materials Pearlstick® 45-60/03 Polycaprolactone based TPU Pearlstick 45-60/03 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a medium thermoplasticity level.Solu.. |
|||
Brookfield Viscosity | 200 - 1800 cP | 200 - 1800 cP | 1% sol. in 1% KCl Brookfield LV 60 rpm spindle n°3; TI-1110 |
Solvay RHODOPOL® 23 Surfactant Description: Rhodopol® 23 is Standard grade Xanthan Gum. It exhibits high pseudoplastic behavior and rapid hydration rate. This grade is registered on the FALCON list of approved substances.Ident.. |
|||
Brookfield Viscosity | 200 cP | 200 cP | RVT Spindle #2, 20 RPM, 23°C, 15% T.S. in MEK |
Lubrizol ESTANE® 5719 Ester Based Thermoplastic Polyurethane Features: High tensile strength, low temperature flexibility, and high adhesion to various substrates such as PET, PVC, and various fabrics.Uses: Fabric coating and audio tape binder, inks and solut.. |
|||
Brookfield Viscosity | 200 cP | 200 cP | / 6 rpm; spindle #2 |
Abatron AboCoat 8204-15/AboCure 8204-15 Epoxy Coating AboCoat 8204-15 is a flammable light-blue liquid resin. AboCure 8204-115 is a flammable clear amber liquid converter. AboCoat 8204-15/AboCure 8204-15 is a dielectric coating for high chemical, solve.. |
|||
Brookfield Viscosity | 200 - 600 cP @Temperature 20.0 °C |
200 - 600 cP @Temperature 68.0 °F |
Brookfield RVT spindle 2.2 RPM |
C.O.I.M. FILCO® 352 Unsaturated Bisphenolic Polyester Polymer for Glass Fiber Sizing Description: Unsaturated Bisphenolic Polyester Polymer for Glass Fiber SizingGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in .. |
|||
Brookfield Viscosity | 200 - 750 cP | 200 - 750 cP | RVF #2 sp @ 20 rpm @ 80°F |
3M Fastbond™ 30-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |
|||
Brookfield Viscosity | 200 - 400 cP | 200 - 400 cP | LVF Spindle #2 @ 30 rpm |
3M Scotch-Weld™ FLX300 Flexible Instant Adhesive 3M™ Scotch-Weld™ Flexible Instant Adhesive FLX (formerly PR851) is formulated for extended resistance to impact, vibration, stress, peel, and humidity applications. It is faster curing than 3M™ S.. |
|||
Brookfield Viscosity | 200 - 400 cP @Temperature 23.9 °C |
200 - 400 cP @Temperature 75.0 °F |
Mixed; ASTM D2393 |
BCC Products BC 8086 Urethane Casting BC 8086 is a rapid setting, low viscosity, polyurethane casting system. It exhibits a working life of 45 seconds and obtains a demoldable hardness at 7 - 10 minutes. Some of the features include: no.. |
|||
Brookfield Viscosity | 200 - 900 cP | 200 - 900 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4470 SBR Latex ROVENE® 4470 is a carboxylated styrene-butadiene emulsion that has a very firm hand with outstanding strength properties. This binder is able to accept high filler loads of calcium carbonate, clays.. |
|||
Brookfield Viscosity | 200 - 900 cP | 200 - 900 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4475 SBR Latex ROVENE® 4475 is a carboxylated styrene-butadiene emulsion that has a very firm hand with outstanding strength properties. This binder can accept high filler loads of calcium carbonate, clays, and a.. |