MarkeTech AN 180 Aluminum Nitride Ceramic Substrate, 99% Purity

Category Ceramic , Nitride
Manufacturer MarkeTech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MarkeTech AN 180 Aluminum Nitride Ceramic Substrate, 99% Purity.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 5.5 x 3.6 in. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 µm polished.
Physical Properties Metric English Comments
Density >= 3.26 g/cc
>= 0.118 lb/in³
Mechanical Properties Metric English Comments
Flexural Strength >= 300 MPa
>= 43500 psi
Thermal Properties Metric English Comments
CTE, linear >= 4.20 µm/m-°C

@Temperature 20.0 °C
>= 2.33 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity >= 170 W/m-K
>= 1180 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
Dielectric Constant 8.7

@Frequency 1e+6 Hz
8.7

@Frequency 1e+6 Hz
Dielectric Strength >= 15.0 kV/mm
>= 381 kV/in
1 MHz
Dissipation Factor 0.00030 - 0.00070

@Frequency 1e+6 Hz
0.00030 - 0.00070

@Frequency 1e+6 Hz