Material Notes:
Bismuth germanate is intrinsic scintillation material with high absorption power. Due to its high effective atomic number and high density, BGO is a very efficient gamma absorber with high photo effect fraction which results in a very good photo peak to Compton ratio. BGO detectors are preferred for medium and high-energy gamma counting and high-energy physics applications.Data provided by the supplier, MarkeTech International.
Physical Properties Metric English Comments
Density 7.13 g/cc
0.258 lb/in³
Mechanical Properties Metric English Comments
Hardness, Mohs 5.0
5.0
Thermal Properties Metric English Comments
CTE, linear 7.00 µm/m-°C
3.89 µin/in-°F
Melting Point 1050 °C
1920 °F
Descriptive Properties Value Comments
Crystal Structure Cubic
Hydroscopic? No
Luminescence: Afterglow <0.005%
at 6 ms
Luminescence: Decay Constant 300 n/s
Luminescence: Integrated Light Output 15-20
NaI:Tl = 100
Luminescence: Photon Yield 2 to 3
300K; 10<sup>3</sup> pH/MeV
Luminescence: Radiation Length 1.1 cm
Luminescence: Wavelength of max emissions 480 nm