Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 7.00 µm/m-°C @Temperature 20.0 °C |
3.89 µin/in-°F @Temperature 68.0 °F |
|
Pyrotek Pyrite N-14 Refractory Board Pyrotek N-14 is a fiberglass reinforced calcium silicate board specifically developed for the non-ferrous industry. The superior strength and unique formulation of Pyrotek N-14 makes it the preferr.. |
|||
CTE, linear | 7.00 - 25.0 µm/m-°C | 3.89 - 13.9 µin/in-°F | Average value: 15.7 µm/m-°C Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |
|||
CTE, linear | 7.00 µm/m-°C | 3.89 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1105-7751 PEEK, with carbon fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
CTE, linear | 7.00 µm/m-°C | 3.89 µin/in-°F | |
MarkeTech BGO (Bismuth Germanate, Bi4Ge3O12) Scintillator Crystal Bismuth germanate is intrinsic scintillation material with high absorption power. Due to its high effective atomic number and high density, BGO is a very efficient gamma absorber with high photo eff.. |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 20.0 °C |
3.89 µin/in-°F @Temperature 68.0 °F |
|
MarkeTech WCu15 Tungsten Copper Alloy Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st.. |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 25.0 - 600 °C |
3.89 µin/in-°F @Temperature 77.0 - 1110 °F |
|
ICE Steatite L-5 Data provided by the manufacturer, International Ceramic Engineering. |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 20.0 °C |
3.89 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials Niobium Carbide (NbC) Coating High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i.. |
|||
CTE, linear | 7.00 µm/m-°C | 3.89 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1105-7041 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 20.0 °C |
3.89 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Glastic Laminates/Shapes SG-200 Fiberglass-Reinforced Polyester Rod Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. Excellent thermal endurance - used to replace silicone rod. |
|||
CTE, linear | 7.00 µm/m-°C | 3.89 µin/in-°F | ISO 11359-2 |
Menzolit Menzolit® HPC 1200 Unsaturated Polyester UP HPC 1200 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc.. |
|||
CTE, linear | 7.00 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.89 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott G018-090 Dental Glass Remarks: High fluoride and Zn-containing Sr-glassApplication: Glass ionomer cement, CompomerAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacities.. |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 20.0 °C |
3.89 µin/in-°F @Temperature 68.0 °F |
|
Sapco C 220 Steatite Information provided by Sapco. |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 20.0 - 1000 °C |
3.89 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Zircar Refractory Composites RS-99R Refractory Sheet Type RS-99R boards are prefired and are unaffected by moisture. They stay rigid even if saturated with water.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI) |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 20.0 °C |
3.89 µin/in-°F @Temperature 68.0 °F |
|
Zircar Refractory Composites RS-DD Refractory Sheet ZIRCAR Refractory Sheet Type RS-D is a structural high-alumina product supplied in thin sheet form. It is composed of high purity alumina, reinforced with high-alumina ceramic fibers. Refractory She.. |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 1000 °C |
3.89 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories APN-1 Special brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 1000 °C |
3.89 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories BPAP Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 1000 °C |
3.89 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories SAL90 Special High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 1000 °C |
3.89 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories SAL90Z Special High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 7.00 µm/m-°C | 3.89 µin/in-°F | y direction |
Arlon TC350 Glass, PTFE and Micro-Dispersed Ceramic High Thermal Conductivity, Excellent Dielectric Constant Control and Phase Stability with TemperatureInformation provided by Arlon Materials for Electronics (MED). |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 20.0 °C |
3.89 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance S-20B Samarium Cobalt Magnetic Material |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 20.0 °C |
3.89 µin/in-°F @Temperature 68.0 °F |
|
Ceradyne SEMICORE® S1-5B MMPA 16/18 SmCo5 Samarium Cobalt Magnet Magnetic alignment parallel to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Her.. |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 20.0 °C |
3.89 µin/in-°F @Temperature 68.0 °F |
|
Ceradyne SEMICORE® S2-17B MMPA 24/18 Sm2 (CoFeCuZr)17 Samarium Cobalt Magnet Magnetic alignment parallel to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Her.. |
|||
CTE, linear | 7.00 - 8.00 µm/m-°C | 3.89 - 4.44 µin/in-°F | |
Zircar Ceramics MOSI2 Molybdenum Disilicide Heating Element ZIRCAR Molybdenum Disilicide Heating Element Type MOSI2 is an electric element principally containing molybdenum disilicide for use in industrial and laboratory furnaces. Elements fabricated of thi.. |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 20.0 - 1000 °C |
3.89 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Ceradyne Ceralloy® 2710 BeO-SiC Applications:terminationssever wedgesload pelletsabsorbersFeatures: former industry standard for terminations etc.Information provided by Ceradyne Company |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 20.0 °C |
3.89 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance S-22B Samarium Cobalt Magnetic Material |
|||
CTE, linear | 7.00 - 100 µm/m-°C @Temperature 55.0 - 250 °C |
3.89 - 55.6 µin/in-°F @Temperature 131 - 482 °F |
Average value: 20.4 µm/m-°C Grade Count:19 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |