MarkeTech Neodymium Gallium Oxide (NdGaO3) Single Crystal Substrate

Category Ceramic , Oxide
Manufacturer MarkeTech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MarkeTech Neodymium Gallium Oxide (NdGaO3) Single Crystal Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the supplier, MarkeTech International.Developed for deposition of III-V nitrides for LEDs, Lasers, etc. Standard orientation: ; GaN Lattice Mismatch 1.2%.
Physical Properties Metric English Comments
Density 7.57 g/cc
0.273 lb/in³
a Lattice Constant 5.43 Ã…
5.43 Ã…
c Lattice Constant 7.71 Ã…
7.71 Ã…
Thermal Properties Metric English Comments
CTE, linear 4.50 µm/m-°C

@Temperature 20.0 °C
2.50 µin/in-°F

@Temperature 68.0 °F
Melting Point 1600 °C
2910 °F
Electrical Properties Metric English Comments
Dielectric Constant 20
20
Dissipation Factor 0.0030
0.0030