Master Bond EP77M-F Silver Conductive, Fast Curing Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive , Epoxy, Electrically Conductive
Manufacturer Master Bond Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond EP77M-F Silver Conductive, Fast Curing Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond Polymer System EP77M-F is a two component, silver filled, electrically conductive adhesive for high performance bonding formulated to cure very rapidly at room temperature. Unlike the majority of two part, silver conductive epoxy systems, EP77M-F has a one to one mix ratio, by weight or volume. It will set up at ambient temperatures within 5-7 minutes even when mixed in very small amounts.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Processing Properties Metric English Comments
Cure Time 240 - 480 min

@Temperature 23.0 °C
4.00 - 8.00 hour

@Temperature 73.4 °F
Descriptive Properties Value Comments
Color Code "A" Silver; "B" Silver
Mix Ratio By Weight 100/100
Set-Up Time, minutes 5-10
At Room Temperature
Viscosity Smooth Paste
Room Temperature