Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 121 °C | 250 °F | |
Permabond TA435 Toughened Acrylic Adhesive & Initiator PERMABOND TA435 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This adhesive may be used in a variety of structural bonding appli.. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | |
Resinlab® CYNERGY CA6401 Adhesive Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | |
ITW Plexus Plexusâ„¢ MA1023 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works. |
|||
Maximum Service Temperature, Air | 121 °C @Pressure 1.72 MPa |
250 °F @Pressure 250 psi |
|
Garlock 9064 Neoprene Sheet Rubber Gasketing Neoprene (CR)FDA-approved. Exceptional material for food plants, with superior resistance to most all food products; oily and aqueous.Information provided by Garlock Rubber Technologies |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | |
Master Bond EP21LV35Med Two Component, Flexible USP Class VI Epoxy System Master Bond Polymer System EP21LV3/5Med is a two part, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulation and casting that cures flexible. It cures readil.. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | |
Loctite® PRISM® 4212 Instant Adhesive Gel Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | May be used to contain foods during baking above this temperature. |
DuPont Teijin Films Mylar® LB Polyester Film, 48 Gauge (12 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester film designed for use as a component of a lamination. Standard thickness offered include 48, 75, and 92 gauges. Variet.. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | May be used to contain foods during baking above this temperature. |
DuPont Teijin Films Mylar® LBT Polyester Film, 75 Gauge (19 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester film that has been corona-treated to provide superior wetting and adhesion to inks, primers, and adhesives. Standard th.. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | |
DuPont Teijin Films Mylar® RL43 Polyester Packaging Film, 150 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL43 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. Mylar® RL43 is designed to produce stro.. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | |
DuPont Teijin Films Mylar® 850H Polyester Film, 80 Gauge Mylar® 850H (also called Mylar® 850) is a co-extruded, one side amorphous, heat sealable polyester film designed to be used in metallized, print, and lamination applications. This film is suitable.. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | |
3M 470 Electroplating Tape 3M™ Electroplating Tape 470 is a conformable and abrasion-resistant vinyl tape with excellent resistance to most chemicals used in typical electroplating processes.Information provided by 3M |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | Service |
3M 7000FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | Service |
3M 7828 Thermal Transfer Polyester Label Material 3M™ Thermal Transfer Polyester Label Materials are thin profile, gloss polyester label stocks that offer excellent durability and moisture resistance. These label materials utilize 3M™ Adhesive 40.. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | cured 14 days @ 50% RH |
3M AC-350 Class A-1 Aerospace Sealant 3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have.. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | MIL-PRF-81733D |
3M AC-665 Class C-12 Aerospace Sealant 3M Aerospace Sealant AC-665 Class C are two-part, manganese-cured, chromate containing, corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corros.. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | cured 14 days @ 50% RH |
3M AC-736 B-2 Aerospace Sealant 3M Aerospace Sealant AC-736 B-2 is a non-chromate corrosion inhabiting sealants, fast cure, low density two-component, manganese dioxide cure, polysulfide fuselage sealant. These Sealants act as an .. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | |
3M Jet-Weld™ TS-230 Adhesive A warm applied, moisture-curing polyurethane adhesive for wood working, laminating and plastic component assembly. Sprayable/extrudable grade with long set time ideal for bonding a wide variety of p.. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | for 30 mins |
3M Scotch® 265 Fine Line Tape Scotch® Fine Line Tape 265 is a high-performance film backed tape designed for in-mold fine line masking where sharp, clean, gel-coat color separation lines are desired.Information provided by 3M |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | |
3M Scotch-Weld™ MG90-77 UV Medical Grade Light Cure Adhesive 3M™ Scotch-Weld™ Medical Grade Light Cure Adhesive is a single component adhesive that cure to give clear bonds when exposed to appropriate ultraviolet or visible light. It contains a fluorescing .. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | |
3M Scotch-Weld™ TE031 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | |
3M Scotch-Weld™ TE040 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | Long term |
3M 93010LE High Strength Double Coated Tape with Adhesive 300LSE 3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl.. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | cured 14 days @ 50% RH |
3M AC-370 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-370 Class B are fast cure, low density polysulfide sealants suitable for fuel tank and fuselage applications. These two-component, manganese dioxide cured sealants are solven.. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | for 30 mins |
3M 471+ Vinyl Tape 3M™ Vinyl Tape 471+ is a conformable vinyl tape with a versatile rubber adhesive. The moderately translucent backing allows for accurate alignment in simple or complex patterns.Information provided.. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | Long term |
3M 9731RW Double Coated Tape 3M™ Double Coated Tapes 9731 and 9731RW have a firm, silicone pressure sensitive adhesive coated on one side of a polyester film carrier and a high performance acrylic adhesive coated on the other .. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | Operating Temperature |
Devcon Fastmeal™ Epoxy Precision Repair EpoxyComments: High-performance, alumina-filled epoxy putty for making fast, dependable emergency repair to leaks in pipes carrying ores, coal, cement, san and gravel. Cures in 5 m.. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | Long Term |
Quadrant EPP Quadrant LSG PC (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | |
ITW Plexus Plexus™ MA922 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, medium open time.Information provided by Illinois Tool Works. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | cured 14 days @ 50% RH |
3M AC-236 Class A-1/2 Aerospace Sealant 3M Aerospace Sealant AC-236 Class A are brushable, two-component, liquid polysulfide polymer sealant providing excellent fuel tank and fuselage seals. They have outstanding resistance to aviation ga.. |
|||
Maximum Service Temperature, Air | 121 °C | 250 °F | |
Master Bond UV15X-5 One Component High Viscosity UV Curable System Master Bond Polymer System UV15X-5 is one component, non-yellowing, UV curable urethane elastomer system possessing high flexibility and outstanding abrasion resistance. This high viscosity system c.. |