Mateck Neodymium Gallate Substrate, NdGaO3

Category Ceramic , Oxide
Manufacturer Mateck GmbH
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mateck Neodymium Gallate Substrate, NdGaO3.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Substrate single crystals for superconductivity
Physical Properties Metric English Comments
Density 7.57 g/cc
0.273 lb/in³
a Lattice Constant 5.426 Ã…
5.426 Ã…
b Lattice Constant 5.496 Ã…
5.496 Ã…
c Lattice Constant 7.707 Ã…
7.707 Ã…
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C
6.11 µin/in-°F
Melting Point 1600 °C
2910 °F
Electrical Properties Metric English Comments
Dielectric Constant 25
25
Descriptive Properties Value Comments
Growth Techniques Czochralski
Orientation (110)
Orientation Accuracy ( ° ), Max 0.5
Parallelness ( ° ), max 0.02
Polishing standard: one side
Production Method Czochralski grown
Roughness of surface (angstroms), max 30
Scratches none
Standard Size (mm) 10 x 10 x 1 or 0.5
State monocrystalline
Structure orthorhombic
Surface Quality with light microscope without defects
Tolerance of Length (mm) ± 0.1
Tolerance of Thickness (mm) ± 0.05