Material Notes:
BLACK PE2280 is an economy , high tinting strength black masterbatch based on LDPE containing high opacity carbon black. It is designed for use in jet black, high gloss injection molding items, sheets and tubings for general purpose. It is not recommended for use in ultra-film or other film products with high performance requirements.Method of Usage: BLACK PE2280 is designed for ease of dispersion and is therefore suitable for direct addition and mixing with plastic resins in mixer, avoiding pollution and malscattering problems caused by pigment.Range of Application: Black PE2280 is designed for use in LDPE, HDPE, LLDPE, PP, PS, and ABS.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
High Load Melt Index 50 g/10 min

@Load 21.6 kg,
Temperature 190 °C
50 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Descriptive Properties Value Comments
Carrier LDPE
Compatibility LDPE, HDPE, PP and Ethylene copolymer
Pigment Content: Carbon Black (%) 50