Material Notes:
YELLOW PE42089 is a yellow LDPE-based masterbatch containing 30% Bisazo Benzidine yellow pigment, designed for use in polyolefin resins (PE and PP, etc.). Color Index No.:Yellow 83Method of Usage: YELLOW PE42089 is designed for ease of dispersion and is therefore suitable for direct addition and mixing with plastic resins in mixer, free from pollution and malscattering problems caused by pigment.Range of Application: YELLOW PE42089 is designed for use in LDPE, HDPE, LLDPE and PP for production of premium high gloss films.
Physical Properties Metric English Comments
Density 0.990 g/cc
0.0358 lb/in³
High Load Melt Index 45 g/10 min

@Load 21.6 kg,
Temperature 190 °C
45 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Descriptive Properties Value Comments
Carrier LDPE
Compatibility LDPE, HDPE, PP and Ethylene copolymer
Pigment Content 45