Meilian Chemical PE900 BLACK MASTERBATCH

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Meilian Chemical Co.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Meilian Chemical PE900 BLACK MASTERBATCH.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BLACK PE900 is an economy black LDPE based masterbatch containing high opacity carbon black. This product is designed for Injection Molding items, extruded tubings and sheets for general purpose. It is suitable for use in films with low performance requirements and the typical end product is trash bags. But it is not recommended for ultra-films or other film products with high performance requirements.Method of Usage: BLACK PE900 is designed for ease of dispersion and is therefore suitable for direct addition and mixing with plastic resins in mixer, avoiding pollution and malscattering problems caused by pigment.Range of Application: BLACK PE900 is designed for use in LDPE, HDPE, LLDPE, and PP.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
High Load Melt Index 5.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
5.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Descriptive Properties Value Comments
Carrier Recycled LDPE
Compatibility LDPE, HDPE, PP and Ethylene copolymer
Pigment Content: Carbon Black (%) 41